Sulfuric acid dew point corrosion caused by low-temperature flue gas exists extensively in the backend of coal-fired boilers and gives rise to the severe failure of components [1,2,3,4,5,6].As the temperature of the flue gas decreases to 200 °C, 99% of the SO 3 in the flue gas combines with water vapor to form sulfuric acid vapor. After …